Figure 6: Measured XRD intensities from the electroplated Cu RDL film as a function of exposed days: (a) the intensity ratio of I(111)/I(200), (b) the intensity of each I(111), I(200). Note that these stem from the recrystallization and grain growth of the electroplated Cu RDL film with time at room temperature.